How to fix stringing on 3D prints
Stringing is the cobweb of thin hairs that appears where the nozzle travels between two parts of a print. It comes from plastic oozing out while the nozzle moves, and it can almost always be tuned away.
Why it happens
Molten plastic keeps creeping out of the nozzle when it is not printing. Every time the nozzle travels across an open gap, a little of it is pulled into a thread. Three things make it worse:
- Too little retraction: the filament is not pulled back far enough before the move.
- Too hot: runnier plastic oozes more.
- Damp filament: water in the plastic boils in the nozzle and pushes it out. PETG, TPU and nylon pick up moisture fastest.
Tune the retraction
Retraction pulls the filament back before each travel move. Direct-drive extruders usually need about 0.4 to 1.5 mm, Bowden extruders about 2.5 to 6 mm. Start from your printer's own profile and change it in small steps.
Print the retraction test once for each length in its table, changing nothing else, and keep the shortest that leaves no strings. Too much retraction causes its own trouble: gaps where the print restarts, or a jammed extruder.
The setting is Retraction length in the printer or filament settings of Bambu Studio and OrcaSlicer, and Retraction → Length in PrusaSlicer's printer settings.
Lower the temperature a little
Drop the nozzle temperature 5 to 10 °C at a time, staying inside the filament's range. A temperature tower shows the coolest temperature that still gives strong layers. The filament pages list the range the slicers' own profiles use.
Dry the filament
If stringing comes with popping or crackling sounds, a rough surface or tiny bubbles, the filament is damp. Dry it in a filament dryer or the oven setting your dryer's maker gives, and store it in a sealed box with desiccant. No retraction setting fixes wet filament.
Shorter and faster travel
- Turn on Avoid crossing walls (Bambu Studio and OrcaSlicer) or Avoid crossing perimeters (PrusaSlicer), so travel moves stay inside the print where strings are hidden.
- A faster travel speed gives the plastic less time to ooze.
- Wipe while retracting drags the nozzle back over the print as it retracts.
Fine strings that remain can be removed with a quick pass of a heat gun or hair dryer.