TPU print settings and tips
A flexible, rubbery filament for parts that bend, squash and grip. It prints slowly, and a direct-drive extruder handles it much better than a Bowden tube.
At a glance
- Nozzle
- 230–240 °C
- Range to test
- 200–250 °C
- Bed
- 35–50 °C
- Density
- 1.22 g/cm³
- 1 kg of 1.75 mm
- ≈ 341 m
- 1 kg of 2.85 mm
- ≈ 128 m
In each slicer's profile
| Slicer | Nozzle | First layer | Bed | Fan | Max flow |
|---|---|---|---|---|---|
| Bambu Studio Bambu TPU 95A HF @BBL P1S | 230 °C | 230 °C | 35 °C | 100–100% | 12 mm³/s |
| OrcaSlicer Generic TPU @Creality | 240 °C | 240 °C | 35 °C | 100–100% | 3.2 mm³/s |
| PrusaSlicer Generic FLEX @MK4S | 230 °C | 230 °C | 50 °C | 30–50% | 3 mm³/s |
As each slicer ships its profile for a 0.4 mm nozzle (Bambu Studio for the P1S, OrcaSlicer for the Creality K1, PrusaSlicer for the MK4S). The profile named after a brand is that brand's own filament.
Good for
- Bumpers, feet, gaskets and grips
- Phone cases and protective covers
- Flexible keychains and straps
Not the best for
- Fast printing: it buckles in the extruder if pushed
- Multicolour feeders unless the maker says they suit it
Printing it well
- Print slowly; the slicer profiles cap its flow far below PLA's.
- Turn retraction down or off to stop it jamming.
- Dry it before printing: damp TPU strings badly.
Tune it for your printer
Temperature tower · Retraction test · Flow rate test · What a print costs
Questions
What temperature should I print TPU at?
The slicers' own profiles print it at 230–240 °C on the nozzle, within a range of 200 to 250 °C. Print a temperature tower to find the best value for your brand.
What bed temperature does TPU need?
The slicer profiles heat the bed to 35–50 °C.
How many metres are on a 1 kg spool of TPU?
About 341 m of 1.75 mm filament, or 128 m of 2.85 mm, at a density of 1.22 g/cm³.
Why is TPU printed so slowly?
It is soft, so it compresses and buckles when pushed fast. The slicer profiles limit its flow to a fraction of PLA's for that reason.
Can a Bowden printer print TPU?
Harder grades, slowly, often yes. Soft grades need a direct-drive extruder.
Other filaments
Settings from each slicer's own filament profile, checked 2026-11-15.