How to fix warping on 3D prints

Warping is when the corners of a print curl up off the bed. Plastic shrinks as it cools, and if the lower layers cool and shrink while the upper ones are still warm, the edges pull up. Large flat prints, like terrain models and baseplates, show it most.

A first-layer test: squares in the corners and the middle of the bed

Make the first layer stick

  • Clean the plate. Wash a PEI plate with dish soap and water; skin oil is the most common reason prints let go.
  • Use the bed temperature for the material. The filament pages list what the slicers' own profiles use, for example 55 to 60 °C for PLA and 90 to 110 °C for ABS.
  • Check the first layer. A nozzle a little too high leaves round, loose lines that peel. Print the first-layer test.

Add a brim

A brim is a flat border of extra lines round the first layer that holds the corners down, and peels off afterwards. 5 to 8 mm is usually enough. Large terrain bases and anything with sharp corners benefit most.

Cool the right amount

PLA likes its cooling fan, but ABS, ASA and to a lesser extent PETG warp when cooled hard. Their slicer profiles already turn the fan down; leave it that way. Keep draughts away from the printer: an open window or an air conditioner nearby is enough to lift a corner.

ABS and ASA need an enclosure

ABS and ASA shrink much more than PLA. Print them in an enclosed printer and let the chamber warm up before you start. Without an enclosure, large ABS parts warp and can split between layers however good the first layer is.

Help it in the design

Rounded corners warp less than sharp ones. For very large flat models, split them into tiles that print separately; TerraPrinter can split a large area into tiles that fit together.

Otázky

What causes warping in 3D printing?

Plastic shrinks as it cools. When the lower layers cool and shrink while the upper ones are still warm, the corners pull up off the bed.

Does a brim stop warping?

It helps a lot: the extra border holds the corners down. Combine it with a clean bed at the right temperature.

Why does ABS warp more than PLA?

ABS shrinks much more as it cools. It needs a warm bed, little cooling and an enclosed printer.

Další návody

Všechny návody · Hotové mapy · Dárky s 3D mapou